Investigation of the effect of la and ti addition to Mg-4Sn-2Al alloy on microstructure, mechanical and corrosion properties

dc.contributor.authorKurt, Penbe
dc.contributor.authorKurnaz, Süleyman Can
dc.date.accessioned2024-06-13T20:17:53Z
dc.date.available2024-06-13T20:17:53Z
dc.date.issued2023
dc.departmentMeslek Yüksekokulu, Gedik Meslek Yüksekokulu, Biyomedikal Cihaz Teknolojisi Programı
dc.description.abstractIn this study, Mg-4Sn-2Al alloy by weight was produced by gravity casting under a controlled atmosphere. The effect of alloying elements added to this alloy on microstructure, mechanical, and corrosion properties was investigated. Alloying elements were chosen as 2% La, and 0.15% Ti by weight. During the research, SEM/EDS, XRD, tensile, % elongation, hardness, hardening exponent, anisotropy coefficients, fracture surfaces, corrosion rates, and corrosion microstructures of the alloys were investigated. According to the results obtained, Mg-4Sn-2Al-2La and Mg-4Sn-2Al-0.15Ti alloys showed higher mechanical properties compared to Mg-4Sn-2Al alloy. While the ultimate tensile strength for Mg-4Sn-2Al alloy was 131 MPa, it increased to 159 MPa for Mg-4Sn-2Al-2La alloy and 163 MPa for Mg-4Sn-2Al-0.15Ti alloy. At the same time, the strain hardening exponent and anisotropy coefficients of Mg-4Sn-2Al alloy increased with the addition of La and Ti. This shows that the formability of the alloy is improved. In addition, there was not much difference in the hardness values of the alloys. At corrosion rates, the lowest corrosion rate was 11.68 mpy in Mg-4Sn-2Al-0.15Ti alloy, 29.69 mpy in Mg-4Sn-2Al-2La alloy and the highest corrosion rate was 46.60 mpy in Mg-4Sn-2Al alloy. The addition of La and Ti decreased the corrosion rate of Mg-4Sn-2Al alloy.
dc.identifier.doi10.1007/s40962-022-00875-w
dc.identifier.endpage1401
dc.identifier.issn1939-5981
dc.identifier.issn2163-3193
dc.identifier.issue2
dc.identifier.scopus2-s2.0-85138172773
dc.identifier.scopusqualityQ2
dc.identifier.startpage1388
dc.identifier.urihttps://doi.org/10.1007/s40962-022-00875-w
dc.identifier.urihttps://hdl.handle.net/11501/1131
dc.identifier.volume17
dc.identifier.wosWOS:000854415600004
dc.identifier.wosqualityQ1
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.institutionauthorKurt, Penbe
dc.institutionauthorid0000-0002-9242-5692
dc.language.isoen
dc.publisherSpringer Science and Business Media Deutschland GmbH
dc.relation.ispartofInternational Journal of Metalcasting
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.subjectMagnesium Alloys
dc.subjectMicrostructure
dc.subjectMechanical Properties
dc.subjectCorrosion
dc.titleInvestigation of the effect of la and ti addition to Mg-4Sn-2Al alloy on microstructure, mechanical and corrosion properties
dc.typeArticle

Dosyalar

Orijinal paket
Listeleniyor 1 - 1 / 1
Küçük Resim Yok
İsim:
Tam Metin / Full Text
Boyut:
2.86 MB
Biçim:
Adobe Portable Document Format